Bruker Hysitron TI-900 Nanoindenter

The Bruker Hysitron TI-900 nanoindenter measures the hardness, modulus and other mechanical properties of micro-to-mesoscale, structures, thin films, and coatings. 

It can apply forces of up to 1.5 N to a sample through probes of specific geometries while precisely measuring the force applied to and deformation of a sample.

Specifications:

  • Displacement noise floor – 1 nm
  • Load noise floor – 1 mN
  • Max load – 14 mN standard head, 1.5 N High-load
  • Tip geometries:
    • Standard Head: Berkovich, Cube Corner, 30- mm diam flat punch, 1, 10, 100 mm radius cono-spherical 

High Load:  Berkovich, 20, 50 mm radius cono-spherical – diamond, 50 mm radius cono-spherical - sapphire